After polishing a pot metal part, I plated using flash copper by brush plating. This was to be a strike coat for copy chrome. After plating flash copper, are you supposed to buff to a shine, or directly proceed to copy chrome? I attempted to buff the "smutty" surface, using white on a loose cotton wheel, down to a smooth copper shine, only to watch the smut AND the copper disappear. Any suggestions?
|
|
||||
|
Sounds like you didn't put a thick enough layer of copper on the part, but without all the relevant information, we can't diagnose the problem correctly. Please use our PRS system in the Tech Support section so that we may properly assist you.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Flash Copper Problem | gwjohnso | Plating Pot Metal | 12 | 02-27-2007 11:41 PM |
| Flash copper over pot metal | minord | Plating Pot Metal | 2 | 05-05-2004 09:47 PM |
| Prepartaion for flash copper on pot metal | tperazzo | Plating Pot Metal | 1 | 04-13-2003 12:25 PM |
| Newbie ? on copychome and flash copper? | KevinW | Plating Pot Metal | 3 | 11-08-2002 12:49 PM |