Default zinc over cad??

I have some headlight cups for a car project I am doing and they are cad plated from the factory. I am going to glass bead blast them but i am sure there will be some cad left on them. Can I plate zinc over the cad?

Thanks
Reply With Quote
  #2 (permalink)  
Old 12-21-2007, 10:28 AM
Newbie
 
Join Date: Jan 2002
Posts: 16
68goat
Default Re: zinc over cad??

Thanks to Caswells online tech. Answered my question.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Can you use zinc wire for anode in Zinc Plating (copy cad)? ms042180 Electroplating Questions 2 12-23-2006 02:46 PM
Zinc Die Cast hademes Plating Pot Metal 2 04-25-2005 09:46 PM
removing zinc modadds Electroplating Questions 4 04-11-2005 01:13 AM
Zinc fastener vans90 Electroplating Questions 0 02-25-2005 12:18 AM
Zinc or not? pastorclyde Plating Pot Metal 1 01-14-2004 01:06 PM


All times are GMT -4. The time now is 07:45 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.