We don't sell bronze anodes. Our bronze plating kit uses stainless steel anodes.
__________________
-- Lance Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm Please support the moderators on our site by leaving reputation for their helpful posts. Read more here. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Sand cast bronze, how to continue? | marinesteam | Metal Polishing Questions | 1 | 05-22-2007 11:33 AM |
| Sand cast bronze, how to continue? | marinesteam | Metal Polishing Questions | 1 | 05-22-2007 07:25 AM |
| Bronze over aluminum | hoytheld | Electroplating Questions | 1 | 10-18-2006 12:50 PM |
| Anode size for 20" wheel? / cleaning anode | hefrod | Electroplating Questions | 1 | 09-08-2005 05:28 PM |
| Coloring/finishing Magnesium Bronze | homydog | Other Metal Finishing Questions | 6 | 04-03-2005 03:03 AM |