Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Electroplating Questions

Notices

Electroplating Questions Discussion Board For Electroplating and Electroless plating.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 01-07-2008, 05:33 PM
ccr ccr is offline
Newbie
 
Join Date: Jul 2004
Posts: 2
ccr
Default Removing ano before Electroless nickel

What do I use to remove an type III hard anodizing on alloy before electroless nickel can be applied?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
removing nickel UFpball7 Electroplating Questions 2 07-26-2006 11:11 PM
Removing Electroless finish... mark123 Electroplating Questions 4 05-07-2004 07:22 AM
electroless nickel vs regular nickel Rocky Electroplating Questions 1 07-24-2003 02:12 PM
removing nickel plating from brass? thomaconda Other Metal Finishing Questions 2 02-27-2003 09:36 AM
Removing Nickel Plating drdarvocet Electroplating Questions 5 10-25-2002 07:55 PM


All times are GMT -4. The time now is 05:48 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.