Default Chrome over Gold

Wondering if there is any problem plating chrome directly over gold.

Thanks for any advice.
Reply With Quote
  #2 (permalink)  
Old 01-20-2008, 06:34 PM
KCV6's Avatar
Amateur Metal Finisher
 
Join Date: Apr 2007
Location: Adelaide, Australia
Posts: 205
KCV6 is on a distinguished road
Default Re: Chrome over Gold

I have never done it, but I see no reason why it won't work. If the gold is clean, surface texture you desire (scratches, no scratches, polished or satin) and active you should be able to plate it with anything.

Cheers Mark
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Candy Gold over XTreme Chrome Pictures UrineMachine Powder Coating Questions 7 03-16-2007 07:27 PM
Xtreme Chrome + Candy Gold? UrineMachine Powder Coating Questions 4 02-25-2007 08:37 PM
Gold Plating on Copy Chrome. ppaan Electroplating Questions 1 07-13-2006 11:00 AM
Chrome Plug 'N Plate over gold finish ntd Electroplating Questions 2 06-17-2003 11:04 PM
flexibility of nickle/chrome/gold plate studuff Electroplating Questions 1 02-16-2002 10:45 PM


All times are GMT -4. The time now is 03:21 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.