Old 03-08-2008, 10:39 AM
Zinc Plating Guru
 
Join Date: Jun 2003
Posts: 321
seanc is on a distinguished road
Default Re: What am i doing wrong?? Green drab

Quote:
Originally Posted by MrPontiac View Post
less than 5 sec. in the green drab
How long do the instructions say to immerse it for?

I don't use OD chromate, so don't know the parameters, but 5 seconds sounds nowhere near enough time.
__________________
Seans Zinc Plating page
Reply With Quote
  #12 (permalink)  
Old 03-08-2008, 07:50 PM
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 165
MrPontiac is on a distinguished road
Default Re: What am i doing wrong?? Green drab

The more time i soak it in the deeper the bronze to reddish color it looks, i want to beat this butt im really frustrated right now!!
Reply With Quote
  #13 (permalink)  
Old 03-30-2008, 03:15 PM
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 165
MrPontiac is on a distinguished road
Default Re: What am i doing wrong?? Green drab

Really shocked nobody popping in any replys to this question, everybody else must be having problems with it to??
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Olive Green drab question MrPontiac Electroplating Questions 1 12-15-2007 12:19 PM
Olive drab chromate over commercial zinc drdelano Other Metal Finishing Questions 4 11-14-2007 12:18 PM
Where can I find Flat Olive Drab powder? kcenicola Powder Coating Questions 1 04-16-2007 06:10 PM
Olive drab powder coat callmej75 Powder Coating Questions 3 07-17-2006 04:29 PM
How dark is the olive drab? + zinc question. jbvan Electroplating Questions 4 02-01-2003 01:12 AM


All times are GMT -4. The time now is 05:20 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.