Morning guys last night we were plating with are acid copper here what happen buff out the parts a few pits not bad. Started the acid copper for 20 min parts was 2x2x5 long 6 amps took the part out and had more pits need help and we were bubbling.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Acid copper not bond on flash copper help | mgcobra | Electroplating Questions | 4 | 10-10-2007 08:51 AM |
| Acid copper | Gabourie | Electroplating Questions | 3 | 09-25-2004 08:42 PM |
| filling small pits with acid copper | danderson | Electroplating Questions | 2 | 08-25-2004 07:55 AM |
| Flash copper vs acid copper for PCB Holes | cdaw | Electroplating Questions | 3 | 02-28-2004 09:47 PM |
| Strike Copper or Acid Copper over Nickel? | mdarr | Electroplating Questions | 2 | 07-13-2003 01:53 AM |