| Notices |
| Electroplating Questions Discussion Board For Electroplating and Electroless plating. |
![]() |
|
|
Thread Tools | Display Modes |
|
|||
|
I'd like to be able to restore some worn metal in gun parts (occasionally without disasembly). Which of these kits would be most durable? Even if I have to re-do it occasionally.
I also have electroless NI but prefer to do this while assembled if possible. Some areas (barrel lugs etc) cannot be removed for conventional plating. Thanks, Greg |
|
||||
|
Copy Chrome would be most durable, with nickel following a close second.
__________________
-- Lance Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm Please support the moderators on our site by leaving reputation for their helpful posts. Read more here. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Durability Question???? | homydog | Powder Coating Questions | 4 | 06-15-2006 11:50 AM |
| Durability problems with polyurethanes | sdold | Powder Coating Questions | 4 | 09-24-2005 08:48 PM |
| High-durability powders | sdold | Powder Coating Questions | 6 | 08-07-2005 11:34 AM |
| 'Plug-N-Plate' durability?? | Zee | Electroplating Questions | 4 | 05-31-2004 11:47 PM |
| Silvachrome durability? | tomg552001 | Electroplating Questions | 0 | 10-23-2003 12:00 AM |