My brother is recovering a Datsun 1200 for racing and asked me to help him restoring the tail light chromes. Because they were broken, I made a mold and used Alumilite for casting it.
To give the chrome aspect I tried several kinds of paints with no success. Then I found Caswell and see that there is other solutions to chroming. So, all this to make a "simple" question, is it possible to use the Caswell products to chrome plastic parts made of Alumilite? If so, what is the best solution? Thanks in advance for your help. |
|
||||
|
Yes it is possible, although not the easiest thing for beginners to do.
If you want a REAL chrome plate, you'd need a triple chrome kit. http://www.caswellplating.com/triple.htm Otherwise, you can use Copy Chrome, http://www.caswellplating.com/copychrome.htm or Electroless Krome, http://www.caswellplating.com/electroless_krome.htm. If you go this route, you'll also need a copper plating kit. http://www.caswellplating.com/copper.htm Now the hard part....you need to make these parts conductive somehow to plate them. So you need some Conductive Paint. http://www.caswellplating.com/csp24.htm The (somewhat simplified) steps are: 1. Conductive Paint 2. Copper Plate 3. Buff 4. Nickel, Copy Chrome or Elec Krome 5. Real Chrome if desired.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|
I finally received the "Electroless Krome! Plating Kit", "Copper Plating Kit 1" and the "Copper Powder" ( picture in http://www.geocities.com/TimesSquare/4545/plating.jpg ) but it looks something is missing. Am I right?
About the plating process, where do I start? "The Complete Manual" has all types of plating and I don't know which I have to use and where to start. Any advices? Thanks. |
|
||||
|
We can't answer product support questions in this forum.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| copy chrome vs triple chrome plating | splbnd27 | Electroplating Questions | 18 | 06-21-2006 07:35 AM |
| Plating Problem grey finish from chrome plating | tshirah | Electroplating Questions | 2 | 08-13-2005 12:08 AM |
| Wanted: Chrome plating in Bay Area (North Cal) | olaf_sc | Services Offered/Wanted | 1 | 11-19-2003 11:22 AM |
| Plating Chrome over Brass | mojobari | Electroplating Questions | 3 | 10-29-2002 03:28 PM |
| Repairing rusted chrome plating | Angel | Electroplating Questions | 2 | 04-19-2002 10:13 AM |