    I picked up an old motorcycle. The previous owner had cleaned the inside tank rust with muriatic acid. Some spilled on the exterior triple chrome plate. It looks as if it ate through the chrome and stopped at the nickel layer, although I am not sure of this. Is my guess correct, and can I plate copy chrome onto the damaged area and get a reasonable repair?

    Thanks
    Robert
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,793

    That's probably likely. Yes, you should be able to use Copy Chrome to repair the damaged area.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. triple chrome vs. nickel/chrome vs. copy chrome
    By spectraflamed in forum Electroplating Questions
    Replies: 4
    Last Post: 01-21-2007, 10:07 AM
  2. copy chrome vs triple chrome plating
    By splbnd27 in forum Electroplating Questions
    Replies: 18
    Last Post: 06-21-2006, 07:35 AM
  3. Pros and Cons between CopyChrom and Triple Chrome
    By Jezella in forum Electroplating Questions
    Replies: 0
    Last Post: 01-29-2005, 05:56 AM
  4. Triple chrome kit or copy chrome
    By pointer66 in forum Electroplating Questions
    Replies: 1
    Last Post: 07-30-2003, 02:29 PM
  5. Hard chrome vs triple chrome
    By butters in forum Electroplating Questions
    Replies: 1
    Last Post: 02-19-2003, 11:35 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1