Question Platinum/Titanium dioxide plating on SS

How can this be accomplished?
What do I need & how do I do it?

I need this for a electrolysis test to produce Hydrogen!
Reply With Quote
  #2 (permalink)  
Old 08-17-2008, 02:26 PM
Newbie
 
Join Date: Aug 2008
Posts: 3
aticama is on a distinguished road
Default Re: Platinum/Titanium dioxide plating on SS

Why would you want this? berto
Reply With Quote
  #3 (permalink)  
Old 08-18-2008, 12:32 AM
CarWiz's Avatar
Experienced Metal Finisher
 
Join Date: Sep 2005
Location: South Texas
Posts: 380
CarWiz is an unknown quantity at this point
Default Re: Platinum/Titanium dioxide plating on SS

Quote:
Originally Posted by vaageng View Post
How can this be accomplished?
What do I need & how do I do it?

I need this for a electrolysis test to produce Hydrogen!
Might be a little hard and expensive to do at home. Besides, you don't need all that to produce hydrogen gas. You can use water and table salt to create an electrolyte. Passing a DC current through two electrodes submersed in the electrolyte will produce hydrogen gas at the negative electrode.

What's going on with you two? Running late on a summer project for school?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Anybody need titanium? acidrain Anodizing Questions 9 06-02-2006 11:37 AM
Platinum plating lphurley Electroplating Questions 2 02-02-2005 06:08 PM
Looking for Titanium Nitride plating ACinVA Services Offered/Wanted 6 06-15-2004 09:58 AM
Platinum plating / vermeil jesz Electroplating Questions 0 08-03-2003 08:30 AM
removing/adding platinum/palidium/rodium plating Mutant Electroplating Questions 0 05-08-2003 09:23 PM


All times are GMT -4. The time now is 05:59 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.