Hey guys
I'm thinking of purchsing the 2 gallon triple chrome kit for some small parts on my motorcycle. I have seen some cars around that look like they have chrome in their paint jobs (like they've had a section chromed and painted around it). Is this possible? Also, is it possible to chrome plate plastics (the cowlings on my motorbike)? I thought about coating the areas with conductive copper paint first and then chroming? Thanks |
|
||||
|
Yeah, the chromed areas are probably not actually a chrome plate - could even be powder coated??
Yes, it's possible to chrome plastic, although not recommended for a beginner. See http://www.caswellplating.com/csp24.htm
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| plating non metal surfaces (plastics for instance) | bigdave | Electroplating Questions | 4 | 06-22-2008 10:26 PM |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 10:11 AM |
| plating and size power? | chromo | Electroplating Questions | 7 | 01-18-2003 03:52 AM |
| Electroless Krome plating Q's | chcarver | Electroplating Questions | 1 | 10-10-2002 11:00 PM |
| Chrome Plating Plastics and Die Cast Metals? | nunnc | Electroplating Questions | 1 | 05-21-2002 03:45 PM |