I am planning on purchasing a plug 'n plate nickel plating kit and was wondering how much surface area the 8 oz of nickel plating solution will cover? I repair antique toy trains and need to plate side rods and small screws, etc.
I am planning on purchasing a plug 'n plate nickel plating kit and was wondering how much surface area the 8 oz of nickel plating solution will cover? I repair antique toy trains and need to plate side rods and small screws, etc.
Sorry, I didn't check the knowledge base before posting. Here's what it says:
At an average thickness the kits will plate approximately:
4oz Gold - 0.5 - 1 sq ft
4oz Silver - 1 sq ft
8oz Nickel - 2 sq ft
8oz Copper - 2 sq ft
8oz Copy Chrome™ - 2 sq ft
8oz Bronze - 2 sq ft
8oz Tin - 2 sq ft
4oz Brass - 1 sq ft