I just got your Electroless Krome kit and I'm going to use it to "Krome" some brass pieces. The question I have is, after I electroless Krome my brass pieces, can I then gold plate them with my existing cyanide based pen plater that I already have?
Will gold plate directly onto a "Krome" finish? Thanks for any info. |
|
||||
|
Yes - gold will plate directly over the E-Krome finish.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Electroless Krome question | scott1 | Electroplating Questions | 1 | 10-04-2003 10:29 AM |
| Black Krome over Electroless Krome? | athomas | Electroplating Questions | 2 | 08-26-2003 02:49 PM |
| Electroless Krome is yellow? | stevec | Electroplating Questions | 3 | 09-17-2002 04:04 PM |
| Electroless Krome Question | mstrayer1 | Electroplating Questions | 1 | 06-26-2002 12:11 PM |
| Electroless Krome | brich | Electroplating Questions | 1 | 12-10-2001 06:25 PM |