    I am kind of new to the world of polishing. I just polished a hub cap made of stainless. First I used black on a sissal wheel after I used white on a regular wheel now I have very fine scratches almost polished out. What would be the next step to get a finely polished peice? I am not looking for shear perfection.

  2. #2
    Rasper is offline Experienced Metal Finisher
    Join Date
    Aug 2006
    Location
    Huatulco, Mexico
    Posts
    360

    Default Re: Stainless

    The scratches are probably from the black compound on the sisal wheel. If you don't have any stainless compound, I would go back and use the black on a cotton buff, (not the same buff you are using for white), until you don't see any scratches, then use the white again. After using the black on a cotton wheel you should see no scratches. Then the white will just add to the shine.

    R

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Stainless
    By donafams in forum Powder Coating Questions
    Replies: 6
    Last Post: 03-15-2010, 11:19 PM
  2. stainless looking finish
    By jaloi in forum Electroplating Questions
    Replies: 1
    Last Post: 12-18-2006, 06:56 PM
  3. How to tell stainless?
    By mpierich in forum Metal Polishing Questions
    Replies: 7
    Last Post: 06-19-2006, 03:51 PM
  4. Stainless
    By mpierich in forum Metal Polishing Questions
    Replies: 11
    Last Post: 12-07-2005, 08:57 AM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •