    I am wanting to polish some aluminum tubing. I have read in several places here about using tripoli to cut through the crud to get a good finish. I have also read about using the brown and white compounds. My question is: Where do you guys buy this stuff? I have looked at Autozone, Advance Auto, O'Rielly, and NAPA. It seems none carry it. I have looked at their online catalog as well as visiting in person. They know of it and have said they get inquiries about it but they don't carry it. Where do you find it?

    I know you guys will know.

  2. #2
    baz
    baz is offline Metal Finishing Guru
    Join Date
    Feb 2006
    Posts
    822

    Default Re: Buying Tripoli compound

    Quote Originally Posted by cpowellpumphrey View Post
    I am wanting to polish some aluminum tubing. I have read in several places here about using tripoli to cut through the crud to get a good finish. I have also read about using the brown and white compounds. My question is: Where do you guys buy this stuff? I have looked at Autozone, Advance Auto, O'Rielly, and NAPA. It seems none carry it. I have looked at their online catalog as well as visiting in person. They know of it and have said they get inquiries about it but they don't carry it. Where do you find it?

    I know you guys will know.
    since you are on CASWELL's forum maybe you should start by CASWELL'S site you will find all the buffing compound you need as well as everything else you need to start polishing.
    Plating Kits Electroplating Kits Aluminum Anodizing Kits Powder Coating Systems Metal Polishing And Buffing Supplies - Caswell Inc.

  3. #3
    lcaswell's Avatar
    lcaswell is offline Caswell Inc President
    Join Date
    Jan 2001
    Location
    Lyons NY USA
    Posts
    643

    Default Re: Buying Tripoli compound

    The Tripoli is the brown compound listed here - Caswell Inc. - Standard Buffing Compounds
    --
    Lance Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.

  4. #4
    cpowellpumphrey is offline Amateur Metal Finisher
    Join Date
    Aug 2010
    Location
    Gulf Coast near Houston
    Posts
    73

    Default Re: Buying Tripoli compound

    Thanks for the pointers guys. Since I'll be buying some dye I'll also pick up some compound too.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Buying Sulpheric Acid
    By westsidemachine in forum Anodizing Questions
    Replies: 1
    Last Post: 07-02-2010, 12:24 PM
  2. Building VS buying..
    By welterracer in forum Oven Building Forum
    Replies: 1
    Last Post: 02-27-2009, 08:12 AM
  3. Having a hard time removing Tripoli from polished raw aluminum
    By dammann in forum Metal Polishing Questions
    Replies: 4
    Last Post: 11-01-2008, 12:34 PM
  4. buying chemicals
    By paintballkidz in forum Anodizing Questions
    Replies: 10
    Last Post: 10-27-2007, 01:20 AM
  5. removing tripoli
    By mh in forum Anodizing Questions
    Replies: 6
    Last Post: 09-02-2006, 02:09 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •