Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Metal Polishing Questions

Notices

Metal Polishing Questions Discussion Board For metal polishing questions.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 02-06-2004, 01:00 PM
Newbie
 
Join Date: Feb 2004
Posts: 3
hptech1
Default Polishing Aluminum Alloy Wheels? Update After & Before

I'm a Newbie, to the Caswell site. Very well done informative site. I can't leave.

I have some 17" American Eagle 077 polished wheels. They have a milky gray haze from I presume going thru the car wash.

I want to bring the lustre and shine back to them. What kit should I purchase to do this? There are two kits I noticed. One involves sanding and stripping and the VHT compound. The other just involves polishing with the Brown & Black bricks Sisal and White polish.

I just want some hints and tricks from the experienced polishers on this forum.

Thanks in Advance Kevin


Before

After
Reply With Quote
  #2 (permalink)  
Old 02-06-2004, 11:47 PM
skiddz's Avatar
Experienced Metal Finisher
 
Join Date: Dec 2003
Location: So. CA
Posts: 253
skiddz
Default

You might be able to get away with a loose cotton wheel and some white compound.. A little more aggressive approach would be a sewn wheel and some brown followed by the loose/white combo.

Are they currently clear coated or anodized? If so, you'll need to strip 'em before buffing.

Check out the online buffing manual for tips on procedures...

Good luck!!
Reply With Quote
  #3 (permalink)  
Old 02-09-2004, 02:47 PM
Newbie
 
Join Date: Feb 2004
Posts: 3
hptech1
Default

Thanks Skiddz. I'll let you know how they turn out.
Reply With Quote
  #4 (permalink)  
Old 02-18-2004, 10:14 AM
Newbie
 
Join Date: Feb 2004
Posts: 3
hptech1
Default

ttt
Reply With Quote
  #5 (permalink)  
Old 08-06-2007, 10:35 AM
Newbie
 
Join Date: Aug 2007
Posts: 9
alumamike is on a distinguished road
Default Re: Polishing Aluminum Alloy Wheels? Update After & Before

Try a product called WHITE DIAMOND it works good on uncoated aluminum wheels
I think there website is whitediamond.com
Reply With Quote
  #6 (permalink)  
Old 08-06-2007, 11:24 AM
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 439
jrow will become famous soon enoughjrow will become famous soon enough
Default Re: Polishing Aluminum Alloy Wheels? Update After & Before

hptech1,

Try using a "clay bar" before you go to any mechanical means on polishing. Then use a good Mag wheel polish.

John
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
Need help polishing my polished aluminum wheels suparida Metal Polishing Questions 12 09-02-2005 09:08 AM
Need Help Polishing aluminum Wheels. mattyp Metal Polishing Questions 13 06-14-2004 08:44 PM
A ? regarding polishing aluminum wheels... geotexZ71 Metal Polishing Questions 4 04-25-2003 08:12 AM
Polishing aluminum motorcycle wheels emprcyrul Metal Polishing Questions 7 02-15-2003 10:28 AM


All times are GMT -4. The time now is 05:37 AM.