I totally agree and know that an anodized finish is simply a chemically finished aluminum surface. What I am struggling with is the clear coat or clear powder coating that has been applied afterwards.
skiddz, for how long do you leave in on? Do you place it in the sun to "bake" or not needed? Thanks! |
|
|||
|
bigfishon1 when you use oven cleaner I found it worked best to heat the metal your working on before hand. When I did my atv rims I just took my heat gun to them first. I did do 1 whitout heating it to see what would happen and it didn't work so well. U can also use a brass wheel it doesn't put deep scratchs the metal. But oven cleaner and heating up the metal worked the best for me and the fastest. Just read the directions on the oven cleaner it even suggest preheating your oven.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| After 1500g sanding, and black emery, frame has black streak | fizlfry | Metal Polishing Questions | 8 | 04-26-2005 10:09 AM |
| greasless compounds | BUFFMAN | Metal Polishing Questions | 2 | 02-05-2004 12:28 AM |
| greasless compound | spydersac | Metal Polishing Questions | 1 | 08-15-2003 01:13 PM |
| Problems with emery compound | hue | Metal Polishing Questions | 13 | 03-03-2003 09:31 AM |