| Notices |
| Metal Polishing Questions Discussion Board For metal polishing questions. |
![]() |
|
|
Thread Tools | Display Modes |
|
|||
|
Okay to you guys that use this stuff... what am I doing wrong?
I load up a pair of Sisal wheels, let it dry... even for a couple of hours one time. Turn it on, hit a part and *!* gone.... I get about 15 seconds of work out of it. The sisal seems to load on the "threads" sticking out, not the wheel face. Any tips? |
|
|||
|
You could probally clean them up by raking the hell out of them. Because of the nature of sisals and their ability to get really small really quick you should be able to rake off the part with greaseless than use them to polish.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Is greaseless cheating? Plus a ? | berad001 | Metal Polishing Questions | 7 | 06-14-2005 02:05 PM |
| Some newbie questions... | kiwijetpilot | Anodizing Questions | 16 | 03-12-2005 08:18 PM |
| A few newbe questions | thestormfamily | Electroplating Questions | 4 | 06-30-2004 08:54 AM |
| How do you use greaseless? | gagnon | Metal Polishing Questions | 3 | 03-21-2003 05:43 PM |
| greaseless compounds | saiyan7 | Metal Polishing Questions | 4 | 04-12-2002 07:29 PM |