I'm restoring a 70s motorcycle. I have cleaned up and polished
several parts already. LIke the exhaust and header pipes and
they turned out very nice. Now I working on the chrome fenders.
After buffing off the surface rust and crud...I can't seem to the
it back to the Chrome shine? The finish stops at a slightly hazy
non shiney look.... What do I need to get that?
I purchased the jumbo bar starter set and I have pads.
Sisle,cotton sprial and look canton...what am I missing?
I really need to get this polishing chrome thing down. thanks
for any and all help. Kirby
__________________
Kirby Martin
Dallas, Texas
kurbster@swbell.net
Reply With Quote
  #2 (permalink)  
Old 03-12-2004, 12:57 PM
skiddz's Avatar
Experienced Metal Finisher
 
Join Date: Dec 2003
Location: So. CA
Posts: 253
skiddz
Default

You may have buffed the chrome off and could be looking at the nickel (assuming it was triple plated here) or the bare metal itself. I think if it were my parts, I'd have 'em replated..

I had pretty good luck polishing the bluing off my ATVs pipes with a sisal wheel and some black emery followed by white rouge on a cotton wheel, but the pipes were in good shape to start with. The white rouge really brought out the shine again..

Perhaps a little more "oomph" with the loose wheel and white rouge. Are you cutting against the wheel's rotation then coloring with the rotation???
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 04:24 AM
Buffing Bicycle Chrome SLCny Metal Polishing Questions 2 04-10-2004 11:19 AM
Chrome (re)plating question - howto olaf_sc Electroplating Questions 1 07-29-2003 02:00 PM
Hard chrome vs triple chrome butters Electroplating Questions 1 02-19-2003 11:35 PM
Buffing Copy Chrome mr.wagon Metal Polishing Questions 1 10-02-2002 11:12 PM


All times are GMT -4. The time now is 05:33 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.