Default Second attempt to polish

I tried a diffrent method all together. skipped the black and went strait to brown with good results. I still get the cloudyness. in the direction to polish. i think i have to start over...the shine is there in some spots. If I could figure out this cloudy part i think it would be perfectperfect. The sanding is a pain but it's worth it to skip the black. It took me six hours all together. if anyone has a hint let me know id like to get it right before i put it back on...check it out its in the picture album under dgc187....thanks all!! I love polishing!!
Reply With Quote
  #2 (permalink)  
Old 06-24-2004, 12:02 AM
customandsound
Guest
 
Posts: n/a
Default

clean it real good and try this set up :
black / sprial cut motion
brown sprial polish motion
green /loose polish motion
white/loose polish motion

don't use a sisal on soft metal .. they tear it up

i use the bottom of the wheel to get my color and go side to side :
Reply With Quote
  #3 (permalink)  
Old 07-25-2004, 01:55 AM
skiddz's Avatar
Experienced Metal Finisher
 
Join Date: Dec 2003
Location: So. CA
Posts: 253
skiddz
Default

For "haze" removal, ease up on your pressure a bit. I did a large, flat skidplate a few weeks ago that was good but for the "haze". I loaded up a loose wheel with white roughe and let it just barely glide over the surface. All the haze went away.

I was able to duplicate this success on the skid plate's billet clamps as well..
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
polish / paint / chrome near northern NJ nickbee Services Offered/Wanted 3 06-17-2005 01:03 AM
What is the best way to polish magneseum? jtltoy Metal Polishing Questions 3 08-07-2004 11:08 PM
Recommend a good aluminum polish for my current situation! qwik3r Metal Polishing Questions 1 05-04-2004 06:36 AM
Fireman needs to polish Diamond Plate Kaleb Metal Polishing Questions 4 12-28-2003 10:46 PM
Silver polish on 24k gold plate?? chromo Electroplating Questions 3 04-07-2003 06:14 AM


All times are GMT -4. The time now is 05:36 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.