Default Finishing Aluminum

I just finished my first 2 projects,a set of lower legs for a Harley and a Harley top triple tree.Both came out show quality but I finished them with the red compound and it barley made any difference.Am I supposed to finish with a different compound or what.I posted the pictures in the picture forum.Any suggestions anyone?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
using aluminum as a cathode scocklin Anodizing Questions 19 03-31-2007 12:18 AM
Do you have to use flash copper to plate aluminum krsimulis Electroplating Questions 1 07-27-2004 01:32 PM
Cleaning Oxidized Aluminum With Sand Blasting Media? freematt Other Metal Finishing Questions 2 02-23-2004 02:22 AM
HELP! White haze when degreasing polished aluminum! davidh90046 Metal Polishing Questions 2 10-15-2002 01:19 PM


All times are GMT -4. The time now is 05:22 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.