Default to much heat?

this is getting hard to deal with! the more i try the worse it gets. it seems that when i try to buff out scratches i get a haze ang can't get rid of it. it looks like the aluminum is getting to hot and burning. holding the piece at an angle you can see brown in the metal. this is with the emery. and also i see grain in the metal will sanding more get this out? i am not giving up but am very irritated.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Aluninum heat transfer rate. levi Powder Coating Questions 6 10-14-2006 11:05 AM
?1) blast cabinet replacement part ?2) exhaust heat shields upncoming Powder Coating Questions 4 03-21-2005 12:33 PM
heat treated aluminum warchild Powder Coating Questions 2 10-25-2003 08:58 PM
Heat Source mitch_vinton Powder Coating Questions 1 07-31-2002 10:35 PM
Heat effects on Chrome nunnc Electroplating Questions 1 06-16-2002 10:55 PM


All times are GMT -4. The time now is 02:00 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.