Hi,
I have a new bike which has 4" dia, chrome plated, slash cut exhaust tips about 30" long. I've managed to get some small scratches and swirl marks along the top facing surface of the 4" dia tube. I've ordered the Chrome polishing kit to hopefully restore a nice scratch-free finish.

My questions:
I'll be using a variable speed drill with the buffing wheel(s) as I dont want to remove the exhaust. What's the best technique for doing this?

Should I work on just the scratches or buff the entire length of the tube?

Which compounds in what order?

Which wheels?

Thanks!
Reply With Quote
  #2 (permalink)  
Old 11-02-2004, 07:36 PM
Newbie
 
Join Date: Mar 2003
Location: Montreal, Canada
Posts: 19
gagnon
Default

removing scratch on Chrome is almost a impossible job to do. Because the first thing your going to remove is the Chrome after that the scratch. If it's a small scratch use green compound cotton after that Formax blue compound with flannel.

P.S. Remember if you remove the Crome plating from your exhaust it's going to rust where you have no plating so be very careful.


hope this help!
Reply With Quote
  #3 (permalink)  
Old 11-29-2004, 12:15 AM
customandsound
Guest
 
Posts: n/a
Default

a replacement or rechrome will work .. but for the blue on the pises it self emery and a sisal and they are shiney again
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Help polishing out scratches on chrome. . Hantra Metal Polishing Questions 5 07-11-2005 05:11 PM
Removing blistered chrome from aluminum wheels? ozziepartsguy2003 Electroplating Questions 0 12-14-2003 06:26 PM
Removing the chrome surface from aluminum based auto trim jbashaw Metal Polishing Questions 6 10-01-2003 10:20 PM
Removing chrome from brass or base metal watch cases prsager Other Metal Finishing Questions 1 03-20-2003 06:06 PM
Removing small scratches from Chrome mlust Metal Polishing Questions 3 10-06-2002 03:34 PM


All times are GMT -4. The time now is 03:44 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.