I\'m looking for recommendations for clearing rust off a carbon steel sword (chinese dao) that used daily in practice.
Sweat on the blade form regular handling is starting a rust buildup. I started cleaning off the rust with fine emery cloth (600) + WD40, but it\'s not effective. What to use for cleanup ? What to use and how often for protection ? David L. |
|
||||
|
Is there any fine detail in this sword that may be lost if polished?
If not, a Spiral Sewn wheel and white buffing compound should make quick work of re-polishing. I haven\'t tried this on carbon steel, but Coca-Cola does a pretty good job if you just want to dissolve the rust.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| How to plate Nickel over old Nickel when steel shows through | ASHENASH | Electroplating Questions | 3 | 04-22-2005 03:03 AM |
| Plug & Plate a Sword blade? | Blackwinter | Electroplating Questions | 7 | 02-02-2005 11:27 AM |
| Electroless nickel on hardened steel | lathe | Electroplating Questions | 0 | 09-07-2004 11:35 PM |
| Refurbishing steel furniture, polished or brushed look | sethp | Metal Polishing Questions | 3 | 08-06-2003 03:02 PM |
| Electro-chemical Etching of Steel | Fibergeek | Electroplating Questions | 5 | 07-16-2003 07:38 PM |