Send a message via MSN to berndog Send a message via Yahoo to berndog
Default glass blasting

I've been polishing poor shape Alcoa truck wheels for years now,,,always sanding poor ones from 80 grit up to 400,,,been wondering if anyone has ever tried sandblasting with glass,,or anything else & how does it turn out?
Reply With Quote
  #2 (permalink)  
Old 03-10-2005, 11:19 AM
Newbie
 
Join Date: Dec 2004
Location: mn
Posts: 48
clydes is an unknown quantity at this point
Default

blast them then da sand with 180 then go right to your buffing wheels they should turn out fine. works for me. clydes
Reply With Quote
  #3 (permalink)  
Old 08-24-2005, 09:33 AM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: glass blasting

If you use baking soda in your media blaster there is no need to use sand paper this will leave a bright finish with out sanding and will not harm the piece you are working on
due to high heat sand can actualy burn items if you are not careful also sand or bead blasting can leave a dull or gray finish on the item that needs to be polished out before plating
I use soda on everything it works great with very little time at the polisher afterwards
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
sand blasting cabinet...relocated to tips n tricks section duke Powder Coating Questions 15 12-30-2007 11:28 AM
Sand blasting VS glass beating? monster01 Other Metal Finishing Questions 2 09-09-2006 08:28 AM
Sand blasting media to use for surface prep tavo1765 Powder Coating Questions 13 03-18-2005 11:58 PM
Looking for a MASKING product for blasting ops Halliwell1 Other Metal Finishing Questions 3 04-21-2004 07:23 PM
Respirator failed while blasting with glass bead... skiddz Powder Coating Questions 5 01-17-2004 01:36 PM


All times are GMT -4. The time now is 01:34 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.