My chrome wheels seem to have slight rust spots in a few corners (had the bike serviced, and they left it in the rain for a week!!!)
Is there a way to repolish these? They seem to be in great condition other than the rust and a few little scratches. Could someone please tell me how to get rid of these things safely? Thank you very much Can post pics now, so, if a pic would help..... |
|
|||
|
I believe you could use a rust remover with no harm to the chrome to get the stains off. But the rust means there's holes in the plating - no real fix for that except clean 'em good then apply a wax product to coat the spots and keep air and water out. Small scratches you can get out with white rouge but you can't buff too hard or you'll go thru the plating.
|
|
|||
|