  #11 (permalink)  
Old 05-10-2005, 10:06 AM
Amateur Metal Finisher
 
Join Date: Aug 2003
Posts: 87
thesound has a spectacular aura aboutthesound has a spectacular aura about
Default

Little drums? Did you click the link I posted? This isn't the die grinder version of the Dremel that you're thinking of, it's a whole other tool that is basically a vibrating sander. This tool doesn't use sanding drums, it uses different "heads" of various shapes that are interchangeable depending on the shape of the surface you're working with, and there are special length bands of sandpaper in either 80 or 120 grit that slip around the heads like a sheath.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #12 (permalink)  
Old 05-10-2005, 11:13 PM
rides20's Avatar
Amateur Metal Finisher
 
Join Date: Apr 2005
Location: Pennsylvania
Posts: 106
rides20
Default

that's what i meant....."Drum-SHAPED" tubes that fit over the contours...I just bought it at sears hardware to 70 bucks....It's identical to the picture..
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #13 (permalink)  
Old 05-16-2005, 04:09 PM
Metal Finishing Guru
 
Join Date: Aug 2004
Posts: 958
mpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of light
Default

Quote:
Originally Posted by caswell
What our web site this week for our new cartridge rolls.
What happened to the cartridge rolls?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #14 (permalink)  
Old 05-16-2005, 06:23 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

They're coming...we've been very busy shipping out you folk's orders.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #15 (permalink)  
Old 05-17-2005, 08:30 AM
Metal Finishing Guru
 
Join Date: Aug 2004
Posts: 958
mpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of light
Default

Quote:
Originally Posted by caswell
They're coming...we've been very busy shipping out you folk's orders.
Haha, well glad you're doing so well - you better hire more help...when you get them on the website you'll get a lot more orders I'm sure.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #16 (permalink)  
Old 05-17-2005, 11:38 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Ok - here is our initial offering. We can get other sizes if people ask for them.

http://www.caswellplating.com/buffs/cartrolls.html
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #17 (permalink)  
Old 05-17-2005, 12:12 PM
Metal Finishing Guru
 
Join Date: Aug 2004
Posts: 958
mpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of light
Default

Quote:
Originally Posted by caswell
Ok - here is our initial offering. We can get other sizes if people ask for them.

http://www.caswellplating.com/buffs/cartrolls.html
OK great, that's a good start. Your price is excellent! I really need the 240 and 320 ones though, and the tapered ones are much more useful. If you get more tapered ones and finer grits I'll definitely be ordering a ton of them from you.

Thanks.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #18 (permalink)  
Old 05-17-2005, 05:27 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 636
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default

ALSO 1/8" MANDREL FOR DREMEL TOOLS
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #19 (permalink)  
Old 05-18-2005, 09:52 AM
Metal Finishing Guru
 
Join Date: Aug 2004
Posts: 958
mpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of light
Default

Quote:
Originally Posted by pickleboy
ALSO 1/8" MANDREL FOR DREMEL TOOLS
Do they make such an animal? Never seen one.

I have made 1/4" x 1/2" mandrels by chucking a bolt into my drill press and clamping my angle grinder to the table, and turning down a shank on the bolt that way (don't have a lathe). Works pretty good if the setup is careful - maybe you could make your own 1/8" mandrel that way.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #20 (permalink)  
Old 05-18-2005, 11:07 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

We can get 1/8" mandrels, but at the moment we can only get the three grit sizes that we have now. We'll keep looking for some finer stuff for you.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off



All times are GMT -4. The time now is 12:50 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.