Nice pictures...they illustrate the problem very well.
Try the techniques discussed in this post and let us know if they solve the problem. http://www.caswellplating.com/bbs/vi...hp?TopicID=350
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Removing small scratches from Chrome | mlust | Metal Polishing Questions | 5 | 07-30-2008 03:39 PM |
| Black Dye problems/Smears and Streaks | Easttex | Anodizing Questions | 1 | 07-16-2004 10:43 AM |
| SCRATCHES | clockman | Metal Polishing Questions | 5 | 06-08-2004 09:18 PM |
| Stainless steel Scratches | SP4SPD | Metal Polishing Questions | 7 | 01-12-2004 09:42 PM |
| How Do I remove tiny, light scratches from Aluminum? | chem_man3 | Metal Polishing Questions | 17 | 03-04-2003 12:46 PM |