the valve cover .. I glassed beaded Grease less then took a sprial with black tore it up. the recess's i use felt bobs and facer buff's on a air die grinder ...
with the glass bead you can get away with a quick polish the total time on that valve cover from raw to done around 1/2 hr... Customer paid 70.00 to have it done .. that pic don't help it any. i took it with a cheap camera ... |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Copy Chrome on engine parts and plastic, alot of can I's | cgworth | Copy Chrome Kit Customers Only | 3 | 08-29-2005 12:38 PM |
| Seek replate of 2 new Chrome Showerheads in Polished Nickel | bradesp | Electroplating Questions | 1 | 08-03-2005 09:10 PM |
| Aluminium Parts Polished?!? | DirtySouthRT | Metal Polishing Questions | 4 | 07-08-2005 03:55 AM |
| Help cleaning just polished parts | bonesaz | Metal Polishing Questions | 3 | 10-12-2004 06:58 PM |
| Detail chrome plating for show parts!! | GOD12A | Electroplating Questions | 0 | 01-11-2004 11:08 PM |