Default Expander Sanding Wheels.

I've got a pretty good sized polishing project to do and I was wondering if anyone has had any experience with the Expander Sanding Wheels?

Do they gouge if used properly?

Any tips would be greatly appreciated.

John
Reply With Quote
  #2 (permalink)  
Old 07-24-2005, 03:18 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default

jrow
from all i have read here they work good and only gouge if you get to aggressive with the pressure. the problem i have is my machines both spin at 3600 rpm so i have not been able to try one yet. i think the recommended max is around 2400. i also heard that they are best on flat work without a lot of contours. hope this helps
best of luck bro
cliff
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #3 (permalink)  
Old 07-25-2005, 11:10 AM
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 449
jrow will become famous soon enoughjrow will become famous soon enough
Default

Thanks Phil,

I have four bumper guards from a 1952 S.I.A.T.A. to polish and they are in relatively bad shape. The sides are pretty flat so I think i'll give it a go. The only problem I can see is that the leading edges are deeply gouged, I may have to find a way to fill them so I don't change the profile to much.

John
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Need Help Polishing aluminum Wheels. mattyp Metal Polishing Questions 13 06-14-2004 08:44 PM
Cant get compound onto the wheels 1105 Metal Polishing Questions 3 04-28-2004 09:05 AM
Where to buy buffing wheels Holmespolish Metal Polishing Questions 0 04-02-2004 12:52 PM
Polishing truck wheels with minor corrosion karter03 Metal Polishing Questions 0 02-19-2004 03:04 PM
A ? regarding polishing aluminum wheels... geotexZ71 Metal Polishing Questions 4 04-25-2003 08:12 AM


All times are GMT -4. The time now is 04:18 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.