Default First time with greaseless!

Well, I finally got around to buying some greaseless, and I was kinda p.o'ed about it at first. I was using a cylindrical firm felt bob and it really didn't seem to have the "cut" that I was expecting, so I just kept trying. After reloading the bob 4 or 5 times, i found that not only did it last longer, but it seemed to cut better...SWEET!!!!!! it was getting late so after reloading a few more times, i decided to call it a night. Is there anything in particular that I need to look for (besides patience?)......Keep Shinin'...Dave S.
__________________
WWW.DSMETALPROJECTS.COM

Polishing and Motocycle customization
Reply With Quote
  #2 (permalink)  
Old 08-19-2005, 07:04 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: First time with greaseless!

If you can get the part to a buffer and use different wheels and compounds it will help with the speed. My preference is the black/ sisal then brown/loose and even white/cotton. If you start with a good grinding before you start polishing is also a must, but I like flapper wheels and 3M disk. Sometimes you can start with a fine glass or sand in a sand blaster before you start grinding, but the most part is a lot of patience.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Is greaseless cheating? Plus a ? berad001 Metal Polishing Questions 7 06-14-2005 02:05 PM
Another newbie - surface area to anodizing time? kumaichi Anodizing Questions 9 11-07-2004 03:46 PM
distilled vs. tap water and anodize time too short blackcote Anodizing Questions 20 07-12-2004 05:44 PM
Anodizing tank time usao Anodizing Questions 12 03-27-2004 03:06 PM
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 09:06 PM


All times are GMT -4. The time now is 02:35 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.