Default I don't want to polish this so what can i do?

I have decided that i do not want the polished look for my rims. What can i do to clean this wheel up, keep the same color, and look perfect? It's supposed to look like the center cap.

Reply With Quote
  #2 (permalink)  
Old 11-05-2002, 10:48 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Does the center cap have a "brushed aluminum" look? It's hard to tell from the picture. If so, a brightex wheel would do the job. See http://www.caswellplating.com/brightex.htm
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 11-05-2002, 10:56 PM
Amateur Metal Finisher
 
Join Date: Sep 2002
Posts: 51
fosgate99
Default

The wheel has lines in it if that helps. What does brushed look like?
Reply With Quote
  #4 (permalink)  
Old 11-05-2002, 11:08 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Like it has lines in it

I think the brightex wheel will do the job for you.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
polish / paint / chrome near northern NJ nickbee Services Offered/Wanted 3 06-17-2005 12:03 AM
What is the best way to polish magneseum? jtltoy Metal Polishing Questions 3 08-07-2004 10:08 PM
Recommend a good aluminum polish for my current situation! qwik3r Metal Polishing Questions 1 05-04-2004 05:36 AM
Fireman needs to polish Diamond Plate Kaleb Metal Polishing Questions 4 12-28-2003 09:46 PM
Silver polish on 24k gold plate?? chromo Electroplating Questions 3 04-07-2003 05:14 AM


All times are GMT -4. The time now is 04:35 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.