Default Steel motorcycle frame rust question.....

hi all, I'm new here and I've already gotten a lot of very useful info, thanks. I've polished the steel exhaust header pipes on my bike and am very happy with the results so far. I'm thinking of doing the frame, which is an older steel tube design. I'm wondering how quickly this will rust if I polish it. will it be similar to my polished SS muffler and the polished header pipes as far as upkeep and corrosion prevention, or is the frame likely made of a different type of steel that will rust more readily. will a monthly hit of Mothers be enough to keep it looking good? Climate is Northern California, and the bike never sees any rain use/is stored in a garage.

thank you!

brian
Reply With Quote
  #2 (permalink)  
Old 11-08-2002, 12:58 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Steel will obviously rust faster than Stainless, but if you take care of it as you describe, you shouldn't have a problem. A good coat of wax would help greatly.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 11-08-2002, 02:09 PM
Newbie
 
Join Date: Nov 2002
Posts: 3
noob-polisher
Default

Sounds good. The frame is anodized right now, so I'l probably be buying some of your anodize stripper. aftre stripping the finish what grade compounds would you recommend I start with for the polishing.

thanks for your help.

Brian
Reply With Quote
  #4 (permalink)  
Old 11-08-2002, 02:14 PM
Newbie
 
Join Date: Nov 2002
Posts: 3
noob-polisher
Default

ooops, just saw the pick-a-buffer page. looks like all the info I need.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Finishing question on frame.... bairdmotorcycles Metal Polishing Questions 9 06-09-2005 01:09 AM
Motorcycle frame - what the best tool? NOrrTH Metal Polishing Questions 4 12-14-2004 06:06 AM
lots of questions, polishing motorcycle frame nopulse95 Metal Polishing Questions 10 02-11-2004 12:39 AM
Got the kit... Now where do I start!! (Motorcycle frame) fatalerror Metal Polishing Questions 9 04-28-2003 12:07 PM
Frame Polishing Question SICKGIXX Metal Polishing Questions 10 03-18-2003 10:50 AM


All times are GMT -4. The time now is 06:02 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.