Hello,
This might be a dumb question but is there any way to polish regular mild steel? i have a cone-shaped spike for my bike i made out of 20 gauge sheet metal and want to have a shiny base so i can paint over it with transperant red spray paint. It looked alright with a spray chrome under the trans. red but would look much better if the metal was polished and then painted over. Thanks |
|
||||
|
Well it all depends on what equipment you have to work with and the finish you are looking for .
For a mild carbon steel I use the following a 3500rpm polishing mtr . Rope spiral wheel with black compound cloth spiral wheel with brown compound cloth spiral wheel with white compound loose cotton wheel with blue compound loose cotton wheel for buffing Caswells offers a great online book to help you with this process here http://www.caswellplating.com/buffs/buffman.htm
__________________
Jim Eaton |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| I'm a noob trying to plate sheet metal | USARMYnoob | Electroplating Questions | 1 | 08-03-2005 09:34 PM |
| metal prep question | corybarta | Powder Coating Questions | 2 | 03-09-2005 01:49 PM |
| Question about getting the metal up to 400 degrees... | Bud | Powder Coating Questions | 5 | 06-08-2004 01:52 AM |
| Lab metal question | NeoMoses | Anodizing Questions | 6 | 12-13-2003 06:33 PM |
| Striation lines while plating sheet metal | mnt mike | Electroplating Questions | 4 | 11-14-2002 04:08 AM |