ok i got it now i resanded with 600 then went at it with black bar then brown then white i found that i realy have to load up the wheel with the white to work but it looks great just some light cut marks under the fluorescent lights but looks great outside will the red bar help this ok now lets talk stainless i got some brake rotors to do any tips
|
|
|||
|
Quote:
|
|
|||
|
Quote:
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| aluminium motorcycle wheels - pc'ing cause failure? | mtnbiker | Powder Coating Questions | 32 | 03-26-2006 10:04 PM |
| Low temp for alum wheels | The_tango | Powder Coating Questions | 3 | 09-25-2003 12:40 PM |
| Motorcycle Wheels | ducatiwv | Electroplating Questions | 1 | 04-20-2003 11:25 AM |
| Polishing aluminum motorcycle wheels | emprcyrul | Metal Polishing Questions | 7 | 02-15-2003 11:28 AM |