Hey guys, I'm close to finished on the centercaps, BUT I have scratches my friends calls them spiderwebs and they seem to come from the buffing wheels I'm using. I'm on the white bar with the spiral sewn wheels. I then tried the white liquid rouge with a soft shammy and it looked better, but you still see small scratches. here are pics:
![]() ![]() I need advice on how to fix this for a present customer? |
|
|||
|
I would also use the loose cotton wheel with the white compound. Apply very minimal pressure to the part. When using a cloth and liquid polish I would also use very little pressure. When finished use a insulator wax on the part.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Removing small scratches from Chrome | mlust | Metal Polishing Questions | 5 | 07-30-2008 02:39 PM |
| SCRATCHES | clockman | Metal Polishing Questions | 5 | 06-08-2004 08:18 PM |
| Stainless steel Scratches | SP4SPD | Metal Polishing Questions | 7 | 01-12-2004 08:42 PM |
| removing scratches and restoring shine? | Augest | Powder Coating Questions | 2 | 01-02-2004 09:00 AM |
| How Do I remove tiny, light scratches from Aluminum? | chem_man3 | Metal Polishing Questions | 17 | 03-04-2003 11:46 AM |