Old 02-11-2006, 01:16 AM
sdold's Avatar
Amateur Metal Finisher
 
Join Date: Jul 2005
Posts: 221
sdold is on a distinguished road
Default Re: is Simple Green safe on aluminum???

Here's the aluminum-safe stuff:

http://industrial.simplegreen.com/ind_prod_ext_mor.php
Reply With Quote
  #12 (permalink)  
Old 02-11-2006, 01:17 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: is Simple Green safe on aluminum???

Yea the stuff is made to clean then wash off, so after you dry the part just put a little polish on it.
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #13 (permalink)  
Old 02-11-2006, 12:47 PM
Newbie
 
Join Date: Nov 2004
Posts: 19
EazyM3
Default Re: is Simple Green safe on aluminum???

thanks for all the good info guys... i'll try the hot water and dishwashing soap in the bathtub while the gf is at work... she'll freak out if she knew i was using it to clean my rims... lol

too bad the simple green aluminum safe is not available to me locally or that be my first choice... it's amazing how much that Easy Off oven cleaner corroded my wheels!!!
Reply With Quote
  #14 (permalink)  
Old 02-11-2006, 03:06 PM
rides20's Avatar
Amateur Metal Finisher
 
Join Date: Apr 2005
Location: Pennsylvania
Posts: 88
rides20
Default Re: is Simple Green safe on aluminum???

Oh yeah!....You should see what a strong mix of sodium hydroxide does!! You've really got to be careful....And now you've got me looking back to all the times i've usesd my tub to clean parts! HAHAAHAHAH
__________________
WWW.DSMETALPROJECTS.COM

Polishing and Motocycle customization
Reply With Quote
  #15 (permalink)  
Old 02-11-2006, 06:45 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,231
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default Re: is Simple Green safe on aluminum???

FYI - Sodium hydroxide (lye) is a main ingrediant in most drain cleaners.
You can always tell the ole lady your cleaning the pipes so you don't get a clog. LOL
SS
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
I found sand blasting aluminum prior to powder coating is a big no-no. mtumbleson Powder Coating Questions 59 04-07-2008 08:37 PM
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 01:16 PM
simple green...... Sid03 Anodizing Questions 3 03-18-2005 01:19 AM
Degreaser - Simple Green? kickn Anodizing Questions 1 09-22-2004 09:50 PM
HELP! White haze when degreasing polished aluminum! davidh90046 Metal Polishing Questions 2 10-15-2002 02:19 PM


All times are GMT -4. The time now is 03:37 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.