Well I got my aluminum wheels polished and they look awsome. I will be at the Detroit Autorama @ Cobo hall this weekend with both my motorcycle, and a friends. I polished the cast aluminum wheels and pulleys on both bikes and am very, very happy with the results. I would like to thank everybody for the suggestions and help. I would probably still be polishing them if not for this board. Anyway enuff a$$ kissing. Here are a few pics of the results. Once again Thank You Very Much!!!!!!!!!