Default polshing stainless

trying to polish some stainless on a race car trailer wet sanded a spot it has some kind of coating on it what is the easiest way to get this coating off thanks
Reply With Quote
  #2 (permalink)  
Old 03-02-2006, 02:18 AM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: polshing stainless

welcome to the forum first off. not doubting you on this but what leads you to think it has a coating on it? some stainless alloys have been passivated to help the outer shell be more corrosion resistant this can create a skin if you will on the outer face of the metal. this may be what you have. if that is the case then just sand it down and start to polish like any other piece of metal. if it has a clear coating on it like some powder coat or paint then it should be stripped with aircraft stripper. then polish as normal. hope this helps bro.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #3 (permalink)  
Old 03-02-2006, 02:27 PM
Newbie
 
Join Date: Mar 2006
Posts: 2
jimmyr is on a distinguished road
Default Re: polshing stainless

when i sanded it, it looks a gray color with shiny stainless underneath, with just trying to buff it you dont get any black coming off the piece thanks
Reply With Quote
  #4 (permalink)  
Old 03-02-2006, 03:46 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: polshing stainless

sounds like it may have been clear coated. i would try the aircraft stripper unless someone with lots of stainless experience hasseen this before and knows different.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Chrome on stainless steel Fick Other Metal Finishing Questions 3 07-05-2005 01:27 PM
blackening 303 stainless?? toku58 Other Metal Finishing Questions 0 01-27-2005 03:45 PM
I need a durable dark finish for stainless. FitzLaughlyn Other Metal Finishing Questions 2 07-17-2003 02:41 PM
Stainless Steel Help, Please rbkemp25 Metal Polishing Questions 4 06-21-2003 07:59 AM
Silver over stainless Rusty Armstrong Electroplating Questions 1 03-25-2002 09:11 PM


All times are GMT -4. The time now is 04:21 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.