Old 03-05-2006, 09:06 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: My recent projects....

try the flash chat...
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #12 (permalink)  
Old 03-05-2006, 09:14 AM
mikekozura's Avatar
Amateur Metal Finisher
 
Join Date: Jan 2005
Location: Monessen PA USA
Posts: 192
mikekozura is on a distinguished road
Default Re: My recent projects....

All man thats cool as h@ll. Enjoy every minute of it. H@ll Kyle's ten already. Thank god for speed channel it dos'nt matter if it has two wheels or four wheels steering wheel or handlebars the motor in it or on it if they race it we watch it. He knows more nascar drivers and numbers then I do. I'd love to freeze him at ten years old for the rest of my life. He's my little buddy.

Dillon, Kyle says hi and ask santa for a Cobra 50 for Christmas.
(Not that many pw50 blue bikes around here anymore)
Reply With Quote
  #13 (permalink)  
Old 03-05-2006, 09:17 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: My recent projects....

Yea I still have my race trailer set up, but its out back and all it does is store my bike and all my gear, every once and while someone will need to use the trailer but thats about it.....
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #14 (permalink)  
Old 03-05-2006, 11:29 AM
BigDog's Avatar
Amateur Metal Finisher
 
Join Date: Dec 2004
Posts: 89
BigDog is on a distinguished road
Default Re: My recent projects....

Quote:
Originally Posted by fly
For those of you who I have talked with about the frame polishing, here are some pictures of two bikes (busa 1300, and gsxr 600). I hope that I can get the picture thing to work so here go's nothing.... Im new at this computer stuff... if their is a easier way, I hope that I will find it.. but for now maybe pics. will show up..
If you can look at the last bike (gsxr 600) frame and you can see that the frame is not like I want it, that finish is with a canton flannel and white, but I tried the canton and blue later and it seemed to do better, so maybe I can get some more pics.... thanks alot, the busa will be ready tuesday so you have to wait on those pics....

Sorry guys but I can't get the picture thing to work......
If anyone can help me move pics from my yahoo account to a post on the forum please help, I will be back in the morning....
I've posted the pics for Fly here: http://forum.caswellplating.com/photopost/showgallery.php?cat=all&si=Fly's
__________________
Jeff B.
Instructions for riding a Warrior: 1) sit on bike, 2) start bike and idle till warm, 3) pull in clutch and put in gear, 4) release clutch and rip on the throttle, 5) {VERY IMPORTANT!!} HOLD THE F*** ON!!!, 6) Enjoy!! Side effects may include whiplash, wrinkle free skin, and an evil smile resembling the "Joker".
Reply With Quote
  #15 (permalink)  
Old 03-05-2006, 12:49 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: My recent projects....

thanks BIGDOG,

does anyone see the frame that I am talking about on the blue/white 600 it is dull looking and I tried the flitz ball and paste but it didn't work. So I am going to try buffing some more. Any suggestions would be apprecieated....
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #16 (permalink)  
Old 03-05-2006, 08:23 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: My recent projects....

i hate to say it bro but the left side looks great to me in the close up. on the right side wide shot it does look less sparkly and it may just be that there is something up with the alloy. not all items will polish up the same. i have run across nozzles before that were the sam maker and they polished different even with the exact same steps. if you are not happy go back to the vented or finger buff and emory and start over from there.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #17 (permalink)  
Old 03-07-2006, 10:18 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: My recent projects....

Yea I think I might have figured it out, I didn't try the blue with the flannel cotton. I tried it on the busa and it worked out good now I have to wait and get the other bike back so that I can fix it....
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #18 (permalink)  
Old 03-07-2006, 10:29 PM
rides20's Avatar
Amateur Metal Finisher
 
Join Date: Apr 2005
Location: Pennsylvania
Posts: 88
rides20
Default Re: My recent projects....

Looks good fly...I noticed "sharpy" marks on the frame..do you typically stop where the plastics cover?
__________________
WWW.DSMETALPROJECTS.COM

Polishing and Motocycle customization
Reply With Quote
  #19 (permalink)  
Old 03-08-2006, 12:04 AM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: My recent projects....

Yea I try to cut down on time and money for me and the customer...
__________________
www.chrome-plater.blogspot.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Recent anodizing failures captmorgan Anodizing Questions 7 07-15-2005 06:37 PM
Visually Curing projects ? garykelly Powder Coating Questions 2 07-27-2004 02:53 PM
First projects tgoode Plating Pot Metal 2 08-03-2003 08:42 PM


All times are GMT -4. The time now is 03:10 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.