first off,i cant believe i found a polishing forum,how cool.my problem:getting a perfect finish on aluminum.i polish big rigs and have no problems with the sanding and cutting part to get the metal shiny,the problem is when i go to the coloring to finish the job.i get a perfect reflection w/depth and clairity,but at different angles/lighting there are kind of a goldish clouds visable on the metal.i seem to have the most trouble with large,flat area's on sheet aluminum.what is it and what causes it?
|
|
||||
|
Could be compound residue? What are you using to color?
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|
I know, a polishing forum has been long overdue. I am polishing motorcycles and the initial cutting part or clearcoat stripping is the hard part for me. Any advice? also, when you are doing big rigs do you clear coat when you are done and if so, does it look good with the clear on the finished piece? Any help you can give me would be much appreciated.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Golf Clubs - How to remove nickel finish prior to refinishin | doctordave | Other Metal Finishing Questions | 3 | 06-03-2005 03:21 PM |
| Newbie, trying to find best way to finish aluminum-LONG POST | chik | Metal Polishing Questions | 6 | 03-14-2005 08:11 PM |
| can we identify this finish? | funkmunky | Electroplating Questions | 3 | 12-15-2004 08:45 PM |
| need help with mirror finish | derekhayes | Metal Polishing Questions | 4 | 07-27-2004 12:22 AM |
| Getting a perfect mirror finish | mole | Metal Polishing Questions | 11 | 02-05-2004 11:20 PM |