I'm looking at some handheld polishers, in particular a Makita 10 amp.
Anyone have experience with these? Do they have enough power to stack 2 or more wheels on it, or is it even possible? Just thinking it would speed up polishing of bigger items. |
|
|||
|
I have that polisher. It is plenty powerful for any polishing job. You cannot put anything more than a 60ply buffing wheel on it though. It is the same one that Caswell used to sell. Great tool. Iknow you can't really see the polish job here, but I used it for this and many other bikes. I would have more pictures of this bike, but I wrecked it shortly thereafter.
![]() |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 12:16 PM |
| on the subject of vibratory polishers | dagobert | Powder Coating Questions | 4 | 01-29-2005 07:48 AM |
| Polishers wanted at Baltimore plating shop | jkurland | Services Offered/Wanted | 1 | 04-10-2004 10:58 AM |
| Handheld polisher? kind of long. | desertjeeper | Metal Polishing Questions | 4 | 03-04-2003 05:16 PM |
| I need aluminum polishers in the area | saiyan7 | Services Offered/Wanted | 1 | 08-12-2002 01:48 PM |