  #41 (permalink)  
Old 02-22-2007, 07:39 AM
Metal Finishing Guru
 
Join Date: Aug 2004
Posts: 958
mpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of lightmpierich is a glorious beacon of light
Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by ptim
So what you are saying is, my covers are not going to get any better and they are as good as they will get.
What happened to the powder-coating idea?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #42 (permalink)  
Old 02-22-2007, 08:30 AM
Newbie
 
Join Date: Jan 2007
Posts: 29
ptim is on a distinguished road
Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by mpierich
What happened to the powder-coating idea?
Its still going to happen, I polish on it a little bit everyday, hoping a silver lining will appear. I have sanded them down some more and they appear to look less "Pitty"......But I think the powdercoating will be easier to keep clean.

The pictures make it look worse than it is, I'm waiting on my powdercoat guy to get back with me.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #43 (permalink)  
Old 03-16-2007, 08:37 PM
Newbie
 
Join Date: Jan 2007
Posts: 29
ptim is on a distinguished road
Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by mpierich
What happened to the powder-coating idea?
I finally got my valve covers polished, they came out pretty good.
Attached Thumbnails
Aluminum Valve Cover Question-pc.jpg  
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #44 (permalink)  
Old 03-23-2007, 03:17 AM
Newbie
 
Join Date: Aug 2006
Posts: 9
mach1canuck is on a distinguished road
Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by ptim
I finally got my valve covers polished, they came out pretty good.
That looks powdercoated
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #45 (permalink)  
Old 03-23-2007, 05:32 PM
Newbie
 
Join Date: Jan 2007
Posts: 29
ptim is on a distinguished road
Default Re: Aluminum Valve Cover Question

Quote:
Originally Posted by mach1canuck
That looks powdercoated
Oops....I meant to say powder Coated, I was thinking one thing and my fingers typed something else, thanks for catching that.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Serious Help Needed, Polishing aluminum valve cover. m3the01 Metal Polishing Questions 29 01-28-2008 12:57 PM
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 01:16 PM
Very Newbie Question: Repairing scratches on aluminum anodized 50 years ago filmfatales Anodizing Questions 2 01-26-2007 04:59 PM
aluminum oxide media question corybarta Powder Coating Questions 5 10-19-2005 12:18 AM
Brand Newbie Aluminum Polishing Question gdsegel Metal Polishing Questions 1 04-25-2003 09:04 AM


All times are GMT -4. The time now is 03:45 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.