Hi Guys, I have been polishing for a few months now and have just reorderd buffs. Most every thing I have polished was solid copper or aluminum and turned out excelent!!

(I too was having the cloud effect and came to the conclusion that it was a combination of temp, and too much compound)
Now I am starting to play with Stainless Steel and Copper sheet metal, but am having trouble with warpage. On the first peice I used a 6" (worn down

sisal with black then Sprial/black, Sprial Brown, Sprial White, Sprial blue. Of course I cought an edge, so back to the plasma cutter and start over.

The pices are about 4' long by 6" wide so I have to do it on a bench with a 3/4 HP Makita 6" hand grinder. Any tips on thin material?
Man I wish these BBS would provide a spell checker