Default Re: Tool Advice

Quote:
Originally Posted by 84Supra
Thanks guys,

I'll be looking for some cartridge rolls and buying some greasless from caswell to help me out. I am assuming a die grinder is the best tool for the rolls? Caswell only sells 120grit rolls, does anybody know of a good source for 320 grit?
maybe if you talk to caswell they could order thev 240 and 320 rolls for you
or find some abrasive supplier in your area.
yes a die grinder is best for the rolls and also for small buffing wheels
check my vrod motor in (polishing pictures ) 90 % of it was done with a die grinder and a orbital air sander

Last edited by baz; 04-04-2007 at 12:39 AM.
Reply With Quote
  #12 (permalink)  
Old 04-04-2007, 11:20 AM
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 449
jrow will become famous soon enoughjrow will become famous soon enough
Default Re: Tool Advice

84Supra,

Try here: http://solutions.3m.com/wps/portal/3...G.x=9&btnG.y=5

John
Reply With Quote
  #13 (permalink)  
Old 04-04-2007, 07:06 PM
Newbie
 
Join Date: Nov 2004
Posts: 33
84Supra
Default Re: Tool Advice

fantastic, thanks for the help guys
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
advice needed please grommit Metal Polishing Questions 4 10-08-2006 12:57 PM
Advice needed on polishing keys Saddlecrew7 Metal Polishing Questions 7 04-16-2006 03:26 PM
dremel type attachments advice grommit Metal Polishing Questions 2 04-06-2006 03:52 AM
Need some advice ... customandsound Powder Coating Questions 3 07-17-2005 01:07 AM
newbie looking for advice badboy71499 Metal Polishing Questions 1 03-03-2004 01:06 AM


All times are GMT -4. The time now is 06:24 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.