Old 04-05-2007, 07:46 PM
Newbie
 
Join Date: Feb 2007
Posts: 35
soccergk is an unknown quantity at this point
Default black or white rouge with aluminum? or both and in which order? need help asap please

which do i use first the black or the white? do i use both with different buffing wheels?
working on this, up to 3k grit
Reply With Quote
  #2 (permalink)  
Old 04-05-2007, 08:39 PM
Newbie
 
Join Date: Feb 2007
Posts: 35
soccergk is an unknown quantity at this point
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

ok just did some searching im going to go with the white because there arent really any scratches left
Reply With Quote
  #3 (permalink)  
Old 04-05-2007, 08:41 PM
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 88
alabama_lowlife will become famous soon enough
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

use black first then white. always use a different wheel for each compound. and if you've got those sanded to 3000 grit, you'll only be stepping backwards with black, just use white and see how it turns out. if it's not good enough, then back up to black.
Reply With Quote
  #4 (permalink)  
Old 04-06-2007, 05:59 PM
Newbie
 
Join Date: Feb 2007
Posts: 35
soccergk is an unknown quantity at this point
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

it kind of looks like the white is putting scratches in it, but the cloudyness is less, is there a fine rouge i should be using?
Reply With Quote
  #5 (permalink)  
Old 04-06-2007, 07:05 PM
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 88
alabama_lowlife will become famous soon enough
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

well, blue is finer than white. you could try it
Reply With Quote
  #6 (permalink)  
Old 04-07-2007, 07:13 AM
Newbie
 
Join Date: Nov 2006
Posts: 16
polierator is on a distinguished road
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

Yes. Blue is the finest rouge so far as i know. I use it as the last rouge.
My steps are brown, green, white and at last blue.
Reply With Quote
  #7 (permalink)  
Old 04-07-2007, 10:16 AM
Newbie
 
Join Date: Feb 2007
Posts: 35
soccergk is an unknown quantity at this point
Default Re: black or white rouge with aluminum? or both and in which order? need help asap please

so should i be using the cutting then the polishing motion? or just the polishing motion?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 03:23 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.