Default Vibratory media questions

Hi,

I recently purchased a small vibratory shaker pot from Harbor Freight. I'd like to clean up some nuts & bolts for a motorcycle restoration I'm doing. I'm not sure as to what kind & grade of media thats best to use for this application. I'm reading / finding out that there are many different grades & types of media . I purchased the only media Harbor Freight had to offer in the store at the time which was a green rust cutting abrasive resin that are triangular shaped. The motorcycle bolts/nuts/small hardware I have are not really rusty , just weathered & aged. I also have some very small aluminum pieces that I'm concerned the rust abrasive media may be to aggressive for. The test lot of used steel bolts/nuts that I ran thru it for about 8-9 hrs. came out OK but are pretty dull looking. I'm look-n for a better finish. Sure would appreciate any advice/tips/etc anyone could share about how to use / applications for some of the other various medias such as walnut & corncob. I see that they come in different grades. Also any advice on media polish or other additives greatly appreciated.

I'm new to the world of aluminum polishing & want to thank you guys & Caswell for the wealth of knowledge thats being shared here. I've learned a lot from this site & have begun purchasing supplies here. Its becoming a fun / interesting new hobby for me. Thanks!!

Critter
Reply With Quote
  #2 (permalink)  
Old 05-23-2007, 01:59 PM
Metal Finishing Guru
 
Join Date: Apr 2005
Posts: 551
jwilbert is a glorious beacon of lightjwilbert is a glorious beacon of lightjwilbert is a glorious beacon of lightjwilbert is a glorious beacon of lightjwilbert is a glorious beacon of lightjwilbert is a glorious beacon of light
Default Re: Vibratory media questions

go to this sight. http://www.caswellplating.com/buffs/...y_tumblers.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
info on blast media Blademan Powder Coating Questions 7 05-18-2007 06:58 PM
Vibratory Tumbler and its media (help) Gunjji Metal Polishing Questions 0 02-16-2006 05:21 AM
Vibratory Tumbler Media hondaman100 Other Metal Finishing Questions 6 08-27-2003 07:38 PM
Media to mirror polish Aluminum in vibratory tumbler hrothgar Metal Polishing Questions 1 07-26-2003 11:32 AM
Vibratory finishing: Continued total failure plus a new clue xiphmont Metal Polishing Questions 2 10-23-2002 02:47 AM


All times are GMT -4. The time now is 07:56 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.