Newbie
 
Join Date: Mar 2003
Posts: 1
Blackvette
Default Cleaning Zinc Plating HELP!!!!

I had my Brake Rotors and Caliper Brackets Zinc Plated last year. I stupidly used one of those caustic brake dust cleaners and it dulled the Zinc to a flat gray color...

Is there a chemical treatment I can use to bring the shine back? Like TarnX or something?

So far I am trying NeverDull Wadding and it messy and time consuming...

I really don't want to have to have them replated all over again..
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Zinc plating on running seal surface? Broke Electroplating Questions 1 12-06-2004 02:52 PM
CopyCad & Zinc failure - electrolyte problems? seanc Electroplating Questions 4 11-08-2004 10:16 AM
NEED HELP QUICK!!! Yellow Zinc Plating Fasteners BryanD Electroplating Questions 1 05-01-2004 01:34 PM
Plating Tank - Zinc aermakov@rogers.com Electroplating Questions 1 03-27-2003 02:38 PM
Zinc Plating Stainless? vnarma Electroplating Questions 1 02-23-2003 11:31 AM


All times are GMT -4. The time now is 04:25 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.