Default creating pits on aluminum

Hi guys. I have polished many parts on my car and now i seem to notice a pattern. If i polish a piece of aluminum to long with the red or white i get these pulls/pits in the aluminum. What's going on? It's really annoying. I have to resand that spot over with paper and it makes my job allot longer. Am i pushing to hard? If i pour water on the metal it boils! Thanks for any help you can provide.
Reply With Quote
  #2 (permalink)  
Old 04-14-2003, 08:56 AM
Amateur Metal Finisher
 
Join Date: Aug 2002
Location: Mississippi Gulf Coast
Posts: 133
marsfrogie
Send a message via AIM to marsfrogie
Default

Those pits were there to begin with most likely. You must first sand them out before you buff the part, or otherwise, use a liquid polish.
Reply With Quote
  #3 (permalink)  
Old 05-09-2003, 10:54 AM
Newbie
 
Join Date: May 2003
Location: pennsylvania
Posts: 12
sparts
Default

if it looks like orange peel use more compound ,or dont let the part get so hot ( maybe try an airway buff helps the part run cooler) or just in the aluminum
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
HELP WITH GETTING OUT PITS IN ALUMINIUM WHEELS!!!! johnnyb Metal Polishing Questions 10 04-27-2005 11:34 PM
Cleaning Oxidized Aluminum With Sand Blasting Media? freematt Other Metal Finishing Questions 2 02-23-2004 02:22 AM
Filling pits in aluminum casting? johnshenry Other Metal Finishing Questions 5 05-11-2003 04:50 PM
HELP! White haze when degreasing polished aluminum! davidh90046 Metal Polishing Questions 2 10-15-2002 01:19 PM


All times are GMT -4. The time now is 02:49 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.